Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 198 MPa
28700 psi
ASTM D882A
DuPont Teijin Films Melinex® 617 Polyester Film, 500 Gauge
Melinex® 617 is a super clear polyester film pretreated on both surfaces with a higher than normal coat weight of T-Sub pretreat for good solvent adhesion.Approvals: UL Recognition - Product has be..
Film Tensile Strength at Break, MD 198 MPa
28700 psi
ASTM D882A
DuPont Teijin Films Melinex® 618 Polyester Film, 500 Gauge
Melinex® 618 is a super clear polyester film, pretreated on one side to promote adhesion. It is a high clarity, non-yellow base with excellent adhesion on the pretreated surface. Used for a wide ra..