Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 527-3
Polimeri Europa Riblene® FF 30 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 30 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 30 is characterized by a good melt strength leading to a good bubble stabilit..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 527-3
Polimeri Europa Riblene® FF 33 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 33 is a high molecular weight low density polyethylene (LDPE), with added slip agent, ideal for blown film extrusion. Riblene FF 33 is characterized by a good melt strength leading to a ..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 527-3
Polimeri Europa Riblene® FF 34 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 34 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 34 is characterized by a good melt s..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 527-3
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit..
Film Tensile Strength at Break, MD 22.0 MPa

@Thickness 0.400 mm
3190 psi

@Thickness 0.0157 in
ISO 527
Premix Thermoplastics PRE-ELEC® ABS 1415 Conductive Thermoplastic Compound
PRE-ELEC® ABS 1415 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® ABS..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 527
Premix Thermoplastics PRE-ELEC® PS 1324
PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 527
Premix Thermoplastics PRE-ELEC® PE 1304  (discontinued **)
PRE-ELEC PE 1304 is a conductive thermoplastic compound based on a blend of PE-LD/PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivi..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ASTM D882
Huntsman PE 1008 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: industrial packaging, frozen food, produce bags, shrink, a..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ASTM D882
ExxonMobil Escorene® LD-141 EVA Shrink Film Resin, FMI  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 2.0% vinyl acetate copolymer film resin with very good toughness and shrink properties. The low melt index gives excellent..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO R527-1
Iran Petrochemical (PCC) 2101TN47 Low Density Polyethylene
LDPE 2101TN47 Shrink FilmThis grade enables high speed production of film without blocking.Information provided by Iran Petrochemical Commercial Co.
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ASTM D882
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film
Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 527-3
Borealis Himod™ FT7293 LDPE for Film
Himod FT7293 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 527-3
Borealis Himod™ FT7294 LDPE for Film
Himod FT7294 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 527-3
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film
LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.LDPE 1022 FH 24 is a slip and anti-block formulated grade.LDPE 1022 FH 24 is suited to many applications in the field of..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ASTM D882
Braskem BC 818 LDPE Extrusion Coating Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Extrusion coating. Information provided by Braskem
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ASTM D882
Braskem CX7020 Cast Film Extrusion Low Density Polyethylene
Smooth or embossed films for diapers, disposable sheets, etc. Films for lamination, Injection-Blow Molding, Foamed applications.Information provided by Braskem.
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ASTM-D882
Braskem CX7020 LDPE Cast Film Extrusion Polyethylene
CX7020 is a low-density polyethylene (LDPE) with excellent processability and low gel content. Those features allow for production of thin and highly uniform films. This product is identified as PE ..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ASTM D882
Braskem PB681/59 LDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Lamination film; general purpose. Information provided by Braskem
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 1184
Carmel Olefins IPETHENE® 100 Low Density Polyethylene
IPETHENE® 100 is a low density polyethylene extrusion grade. It exhibits good impact and puncture resistance, good processability and good ESCR. APPLICATIONS IPETHENE® 100 is used for production..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 1184
Carmel Olefins IPETHENE® 320 Low Density Polyethylene
IPETHENE® 320 is a general purpose low density polyethylene film extrusion grade, containing no additives. It exhibits good mechanical and optical properties. APPLICATIONS IPETHENE® 320 is mainl..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 1184
Carmel Olefins IPETHENE® 322 Low Density Polyethylene
IPETHENE® 322 is a general purpose low density polyethylene film extrusion grade. It contains a medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between ..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 1184
Carmel Olefins IPETHENE® 323 Low Density Polyethylene
IPETHENE® 323 is a general purpose low density polyethylene film extrusion grade. It contains a high level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between me..
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 527-3
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film
LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene..