Polymer Property : Film Tensile Strength at Break, MD = 224.94 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 224.94 MPa
32625 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® HB3 Polyester Film, 200 Gauge
Teijin® Tetoron® HB3 is a super smooth polyester film with a UV absorbing agent, originally designed for green house applications. It has excellent weather-durability, low color and low haze. It i..
Film Tensile Strength at Break, MD 224.94 MPa
32625 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® S Polyester Film, 1000 Gauge
Teijin® Tetoron® S is the designation for a family of clear to hazy polyester films. They are general purpose films having good physical and electrical properties. They also have good chemical and..
Film Tensile Strength at Break, MD 224.94 MPa
32625 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® S Polyester Film, 300 Gauge
Teijin® Tetoron® S is the designation for a family of clear to hazy polyester films. They are general purpose films having good physical and electrical properties. They also have good chemical and..
Film Tensile Strength at Break, MD 224.94 MPa
32625 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® S Polyester Film, 400 Gauge
Teijin® Tetoron® S is the designation for a family of clear to hazy polyester films. They are general purpose films having good physical and electrical properties. They also have good chemical and..