Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 25 µm) PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 30 µm) PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 40 µm) PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 50 µm) PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 25 µm) PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 30 µm) PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 40 µm) PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 50 µm) PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 25 µm) PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 30 µm) PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 40 µm) PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 50 µm) PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 25 µm) PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 30 µm) PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 40 µm) PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 50 µm) PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PL11 Lamination Grade BOPP Plain Film (thickness: 18 µm) PL11 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminating.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PL13 Lamination Grade BOPP Plain Film (thickness: 15 µm) PL13 is a woven bag lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminatin.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PL13 Lamination Grade BOPP Plain Film (thickness: 18 µm) PL13 is a woven bag lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminatin.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PL21 Lamination Grade BOPP Plain Film (thickness: 18 µm) PL21 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. It has excellent dimensional stability, high tensile strength,.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 15 µm) PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 18 µm) PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PP11 Printing Grade BOPP Plain Film (thickness: 18 µm) PP11 is a general, printing grade BOPP plain film. It is transparent and non heat sealable. It has excellent ink adhesion. One side has corona treatment. It is widely used in printing applications.I.. |
|||
Film Tensile Strength at Break, MD | 155 MPa | 22500 psi | ASTM-D882 |
Kinlead PT21 Adhesive Tape Grade BOPP Plain Film (thickness: 60 µm) PT21 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion. Both sides have corona treatment. It is widely used in industrial adh.. |