Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 18.5 MPa
2680 psi
ASTM D882
Petroquimica Triunfo Trithene® TS 7045 LDPE - Film - Plastification
The Trithene TS 7045 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films..