Polymer Property : Film Tensile Strength at Break, MD = 27.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 27.5 MPa
3990 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF250YZ Low density polyethylene
LDF250YZ is a low density polyethylene resin for film extrusion. LDF250YZ has no slip and anti-block additives. LDF250YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..