Film Tensile Strength at Break, MD 241 - 296 MPa
35000 - 43000 psi
ASTM D882
Honeywell Capran® Emblem™ 1000 Bi-Axially Oriented Nylon 6 Film
Description: Capran® Emblem™ 1000 is a 0.40 mil (10 micron) biaxially oriented nylon 5 film with excellent flex crack resistance and superior clarity properties. Applications: packaging appl..