Polymer Property : Film Tensile Strength at Break, MD = 36.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 36.3 MPa
5260 psi
ASTM D882
Lotte Chemical Titan TITANEX® LF2554 Linear low density polyethylene Hexene-1 resin  (discontinued **)
LF2554 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for slot cast extrusion which offers outstanding toughness, extrudability and d..
Film Tensile Strength at Break, MD 36.3 MPa
5260 psi
Kuraray HYBRAR® BF2 Three Layer Blown Film
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb..