Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 30.5 MPa
4430 psi
ASTM D882
ExxonMobil Escorene® LD 319.92 Film Resin  (discontinued **)
Escorene Ultra LD 319.92 is a 9.0 wt% vinyl acetate copolymer film resin, that exhibits superior impact strength and heat sealability.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, MD 30.5 MPa
4430 psi
ASTM D882
LyondellBasell Ultrathene® UE672006 Ethylene Vinyl Acetate Copolymer, Film Grade
Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w..
Film Tensile Strength at Break, MD 30.5 MPa
4430 psi
ASTM D882
LyondellBasell Ultrathene® UE672102 Ethylene Vinyl Acetate Copolymer, Film Grade
Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w..
Film Tensile Strength at Break, MD 30.5 MPa
4430 psi
ASTM D882
LyondellBasell Ultrathene® UE672317 Ethylene Vinyl Acetate Copolymer, Film Grade
Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w..