Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 45.8 MPa
6640 psi
ASTM D882
ExxonMobil LL 1235x70 Cast Film Resin  (discontinued **)
LL 1235x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, MD 45.8 MPa
6640 psi
ASTM D882
ExxonMobil LL 1107x93 Blown Film Resin
Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr..
Film Tensile Strength at Break, MD 45.8 MPa
6640 psi
ASTM D882
ExxonMobil LL 1107x95 Blown Film Resin
Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr..