Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 313.8 MPa | 45510 psi | 25°C; ASTM D882 |
UBE UPILEX VT Polyimide Film Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries.. |