Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 31.9 MPa
4630 psi
ASTM D882
ExxonMobil Escorene® LD 767.MJ Cast and Compounding Film Resin  (discontinued **)
Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical