Polymer Property : Film Tensile Strength at Break, MD = 4750 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 32.8 MPa
4750 psi
ASTM D882
Formosa Plastics Formolene® L62009A Film (Hexene Grade) LLDPE
Hexene Copolymer (High Antiblock)Applications: Blown film applications that don’t require slip.Blown film applications that don’t require slip.Meets all requirements of the U.S. Food and Drug Admi..
Film Tensile Strength at Break, MD 32.8 MPa
4750 psi
ASTM D882
Formosa Plastics Formolene® L62009E2 Film (Hexene Grade) LLDPE
Hexene Copolymer (High slip and antiblock)Applications: Blown film, general purpose filmBlown film, general purpose filmMeets all requirements of the U.S. Food and Drug Administration as specified i..
Film Tensile Strength at Break, MD 32.8 MPa
4750 psi
ASTM D882
Formosa Plastics Formolene® L62009H Film (Hexene Grade) LLDPE
Hexene Copolymer (Barefoot)Applications: Higher AO package for cast and stretch filmHigher AO package for cast and stretch filmMeets all requirements of the U.S. Food and Drug Administration as spec..
Film Tensile Strength at Break, MD 32.8 MPa
4750 psi
ASTM D882
Formosa Plastics Formolene® L62009B Film (Hexene Grade) LLDPE
Hexene Copolymer (Barefoot)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles..
Film Tensile Strength at Break, MD 32.8 MPa
4750 psi
ASTM D882
Formosa Plastics Formolene® L62009X Film (Hexene Grade) LLDPE
Hexene Copolymer (Barefoot)Applications: Cross laminated filmCross laminated filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of..