Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 34.1 MPa | 4940 psi | ASTM D882 |
ExxonMobil Escorene® LD 712.06 Film Resin
(discontinued **) Escorene Ultra LD 712 series is a fraction melt index, 10 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particular.. |