Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 50.5 MPa | 7330 psi | ASTM D882 |
ExxonMobil LL 3404.48 Cast Film Resin
(discontinued **) LL 3404.48 is a hexene medium density polyethylene cast film grade for applications requiring high strength and high stiffness. It can also be used in blown films. Films produced from this resin ex.. |