Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 39.03 MPa | 5661 psi | ASTM D882 |
Dow DOWLEX™ 2027G Linear Low Density Polyethylene For high speed, thin gauge applications Improved stiffness Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |