Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 59.0 MPa
8560 psi
ASTM D882
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy  (discontinued **)
Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol..
Film Tensile Strength at Break, MD 59.0 MPa
8560 psi
Orientation not specified; ASTM D882
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th..
Film Tensile Strength at Break, MD 59.0 MPa
8560 psi
ISO 527-3
Total Lumicene® mPE M 2310 EP Metallocene Polyethylene, Blown Film
Lumicene® mPE M 2310 EP is a second generation metallocene based Linear Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2310 EP can be processed at high output rates with low ext..
Film Tensile Strength at Break, MD 59.0 MPa
8560 psi
ASTM D882
Eastman Eastman 1223 Copolyester
Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card..
Film Tensile Strength at Break, MD 59.0 MPa
8560 psi
ASTM D882
Eastman GSP01 Copolyester for Film and Sheet Extrusion
Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s..
Film Tensile Strength at Break, MD 59.0 MPa
8560 psi
ASTM D882
Eastman Tritan FX100 Copolyester
Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w..
Film Tensile Strength at Break, MD 59.0 MPa
8560 psi
ASTM D882
Eastman Tritan MP100 Copolyester
Eastman Tritan MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation co..
Film Tensile Strength at Break, MD 59.0 MPa
8560 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7105D Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPE Appl..
Film Tensile Strength at Break, MD 59.0 MPa
8560 psi
ASTM D882
Chevron Phillips MarFlex® D139DK Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..
Film Tensile Strength at Break, MD 59.0 MPa
8560 psi
ASTM D882
Chevron Phillips MarFlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..
Film Tensile Strength at Break, MD 59.0 MPa
8560 psi
ASTM D882
Westlake Hifor LT74107-F Polyethylene Film, Using Energx Technology Services  (discontinued **)
Hifor LT74107-F polymer is a high strength and good clarity polyethylene designed for blown film extrusion that contains medium slip, high antiblock and high processing aid additives. Films produced..