Polymer Property : Film Tensile Strength at Break, MD = 6140 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 42.3 MPa
6140 psi
Calculated from mfr's report of 87 N/cm per ASTM D828 and the typical thickness
DuPont™ Nomex® 418 Paper, 8 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..