Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 62.6 MPa | 9080 psi | ASTM D882 |
ExxonMobil NTX™ NTX 101 Super Strength Film Resin NTX 101 is a super strength hexene copolymer LLDPE film resin. Films made from this resin have outstanding toughness properties, especially impact and tear strength, compared to other hexene copoly.. |