Polymer Property : Film Tensile Strength at Break, MD = 65.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 65.1 MPa
9440 psi
ASTM D882
LyondellBasell Alathon® L4903 High Density Polyethylene
ApplicationsALATHON L 4903 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits excellent machine direction tear in an HMW-HD resi..