Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 47.5 MPa
6890 psi
ASTM D882
ExxonMobil EXACT™ 3024 Plastomer for Cast Film Applications
Product Description: Exact 3024 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. It can be used for both monolayer and multilayer coextruded ..