Polymer Property : Film Tensile Strength at Break, MD = 7820 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 53.9 MPa
7820 psi
ASTM D882
Lotte Chemical Titan TITANCEED® mL1061 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL1061 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant, antiblock and slip agent. Films made from Titanceed® mL1061 have outstanding tensile..
Film Tensile Strength at Break, MD 53.9 MPa
7820 psi
ASTM D882
Lotte Chemical Titan TITANCEED® mL1064 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL1064 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL1064 have outstanding tensile, impact and puncture stre..
Film Tensile Strength at Break, MD 53.9 MPa
7820 psi
ASTM D882
Lotte Chemical Titan TITANCEED® mL156 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL156 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt..
Film Tensile Strength at Break, MD 53.9 MPa
7820 psi
ASTM D882
Lotte Chemical Titan TITANCEED® mL216 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL216 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt..
Film Tensile Strength at Break, MD 53.9 MPa
7820 psi
ASTM D882
Lotte Chemical Titan TITANEX® HF1881 High density polyethylene Hexene-1 resin
HF1881 is a pelleted medium molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners and thin films.Advantages: Speci..
Film Tensile Strength at Break, MD 53.9 MPa
7820 psi
Dow Elite® 5400 Linear Low Density Polyethylene
5400 enhanced polyethylene resin is a copolymer produced via INSITE technology from Dow Plastics. It offers extremely high impact resistance, combined with excellent tear, tensile, and optical prop..