Film Tensile Strength at Break, MD 55.49 MPa
8048 psi
ASTM D882
Dow INSPIRE™ D118.01 Developmental Performance Polymer
D118.01 Developmental Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion. Film and sheet produced from this resin offer improved stiffness, heat resistance, ..