Polymer Property : Film Tensile Strength at Break, MD = 8050 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 20.7 - 55.5 MPa
3000 - 8050 psi
Average value: 41.4 MPa Grade Count:3
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..