Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 59.8 MPa | 8670 psi | Calculated from mfr's report of 152 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® E56 Paper, 10 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |