Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 96.5 MPa
14000 psi
ASTM D882
Dow SARAN WRAP™ 18 Plastic Film
SARAN WRAP™ 18 Plastic Film is a clear biaxially oriented monolayer barrier film, designed for chub packaging machines and laminations. It is available in 100 gauge, as single or double would roll..
Film Tensile Strength at Break, MD 96.5 MPa
14000 psi
ASTM D882
Dow Saran® 18L Clear Plastic Barrier Film
Saran™ 18L is a clear biaxially oriented monolayer barrier film, preshrunk for lamination applications. It is available in 75 gauge, as single or double wound rolls.Information provided by Dow