Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 66.3 MPa | 9620 psi | ASTM D882 |
Solvay Specialty Polymers Ajedium™ Films -- Veradel® PES 201 NT Polyethersulfone (PESU) Veradel® PES 201 NT polyethersulfone is a tough, high-strength thermoplastics that are suitable for continuous use up to 356°F (180°C). Veradel® film is resistant to oxidation and hydrol.. |