Polymer Property : Film Tensile Strength at Break, MD = 9910 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 68.3 MPa
9910 psi
ASTM D882
LyondellBasell Adflexâ„¢ Q 401 F TPO Resin
Thermoplastic olefin resin wit slip and antiblock for air quenched blown film, excellent heat resistance, excellent puncture resistance, great tear resistance, FDA acceptableApplications: films requ..