Polymer Property : Timken Test = 25.0 lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Timken Test 11300 g
25.0 lb
ChevronTexaco FM NLGI 1 Grease EP
FeaturesChevron FM Greases EP are high performance, multipurpose food machinery greases that are white in color, odorless, tasteless, and water-resistant. Available in three grades, Chevron FM Greas..
Timken Test 11300 g
25.0 lb
ChevronTexaco ISO 46 Industrial Oil EP
FeaturesChevron Industrial Oils EP are multipurpose oils for industrial service.Chevron Industrial Oils EP are designed to help minimize wear in all types of plant lubrication and also provide long ..
Timken Test 11300 g
25.0 lb
ChevronTexaco ISO 100 Industrial Oil EP
FeaturesChevron Industrial Oils EP are multipurpose oils for industrial service.Chevron Industrial Oils EP are designed to help minimize wear in all types of plant lubrication and also provide long ..