Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized High Impact, Good Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Polymer Resources PC-FR3-D-[color]-3 Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Polymer Resources PPX-GP1-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Extrusion Notes: All physical, mechanical and thermal testing conduc.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (DAM) Information provided by Ravago. |
|||
Tensile Strength, Yield | 55.2 - 82.7 MPa | 8000 - 12000 psi | ASTM D638 |
Alcoa KAMA 2100 Prime Clear OPS, Film
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Fiberfil® J-60/10/FR Polypropylene Homopolymer, 10% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 05012 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES Electrablend® PC C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Spartech PP5410 Glass Fiber Reinforced Homopolymer Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES HiFill® PBT 613 Availability: North AmericaForms: PelletsFeatures: Good Flow and Good ProcessabilityAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES HiFill® PBT E Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Extrusion and Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES HiFill® PP GF10 CC 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES Plastiblend® PC/ABS 8800 Availability: North AmericaForms: PelletsFeatures: High Impact Resistance and High Temperature StrengthProcessing Method: Profile ExtrusionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES Plastiblend® PC/PBT IM 1012 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES HiFill FR® PC FR UG X GY158 Availability: North AmericaForms: PelletsAdditive: Mold ReleaseFeatures: Flame Retardant and Good Mold ReleaseAppearance: GreyInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Clariant Renol PA123 Nylon 66, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Clariant Renol PCSP0008BK Polycarbonate, ESD Protection Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Clariant Renol PCSP0016BL-201 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Clariant Renol PCSP0019 Polycarbonate/Acrylic Alloy Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Asahi Kasei Thermylene® P1-35FM-1374H 35% Glass/Fiber Reinforced Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 55.2 - 82.7 MPa | 8000 - 12000 psi | ASTM D638 |
Alcoa KAMA 1120 Prime AntiFog OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
PlastxWorld Veroplas PA2002MI Nylon 6 general purpose, unfilled, medium impact modified injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 55.2 - 82.7 MPa | 8000 - 12000 psi | ASTM D638 |
Alcoa KAMA 1100 Prime Clear OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |