Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 0.655 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.655 MPa

@Strain 300 %
95.0 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® RT-3615 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation..