Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 1.25 MPa | >= 181 psi | ASTM D412 |
Precision Polymer Engineering S70L Conductive Silicone Rubber Tan coloured, Silicone Rubber, 66-75 °IRHD. Electrically conductive, Silver/Aluminum filled silicone rubber. Equivalent to Mil G 83528 Type D.Applications: Specially compounded to offer excellent .. |