Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 1.41 MPa | >= 204 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7027 Butyl and Halobutyl Rubber General purpose Chlorobutyl; High dampingInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | >= 1.41 MPa | >= 205 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 5861 Fluoro-silicone Fluoro-silicone meeting MIL-R-25988BInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.41 MPa @Strain 300 % |
205 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3740 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding.. |