Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.68 MPa | 244 psi | ASTM D412 |
Polymax® Maxelast® P3908T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 1.68 MPa | 244 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 5353 Nitrile Rubber General purpose NitrileInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.68 MPa | 243 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 7202 Nitrile Rubber Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc. |