Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 10.304 MPa | 1494.5 psi | -36% change after 72 hours @ 250°C; ASTM D412 |
Precision Polymer Engineering Perlast® G70K Perfluoroelastomer Special white compound with wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Recommended f.. |