Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.992 MPa
1594.3 psi
107% Retention, Air Oven Aged 42 days at 121°C
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 10.992 MPa
1594.3 psi
107% Retention, Air Oven Aged 42 days at 121°C
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer
Information provided by Teknor Apex Company