Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.0827 - 0.689 MPa | 12.0 - 100 psi | Average value: 0.229 MPa Grade Count:6 |
Overview of materials for Silicone Foam This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW.. |