Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1040 MPa | 151000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 20% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Tensile Strength, Yield | 1040 MPa @Strain 0.200 % |
151000 psi @Strain 0.200 % |
|
Haynes 25 alloy, room temperature after 20% cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |