Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1041 MPa @Strain 0.200 % |
151000 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, 30% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 1041 - 1048 MPa @Strain 0.200 % |
151000 - 152000 psi @Strain 0.200 % |
|
Latrobe Lescalloy® Jethete M-152 ESR 1.25 RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
Tensile Strength, Yield | 1041 - 1061 MPa @Strain 0.200 % |
151000 - 153900 psi @Strain 0.200 % |
|
Latrobe Lescalloy® Jethete M-152 ESR 6" RCS High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800°.. |