Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 0.724 MPa | >= 105 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7272 Butyl and Halobutyl Rubber General purpose Chlorobutyl; High dampingInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 0.726 MPa | 105 psi | ASTM D638 |
Cheng Yu Plastic 3245 TPE Rubber |