Polymer Property : Tensile Strength, Yield = 1058 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1058 MPa

@Strain 0.200 %
153500 psi

@Strain 0.200 %
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, 3 Part Heat Treatment, 0.062 inch (1.57 mm) Thickness
Tensile and bearing strengths (ultimate and yield) and elongation values reported here are typical for Cold Rolled Sheet, 3 Part Heat Treatment, 0.062 inch (1.57 mm) Thickness samples. Density and m..