Polymer Property : Tensile Strength, Yield = 1085 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1085 MPa

@Strain 0.200 %
157400 psi

@Strain 0.200 %
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Forged Disc, 2 Part Heat Treatment
Tensile strength (ultimate and yield), reduction of area, and elongation values reported here are typical for Forged Disc, 2 Part Heat Treatment samples. Density and magnetic permeability are typica..