Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 11.00 MPa
1595 psi
ASTM D638
ExxonMobil LL 6100 Injection Molding Resin  (discontinued **)
LL 6100 is a narrow molecular weight butene copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in freezer applications ..
Tensile Strength, Yield 11.00 MPa
1595 psi
ASTM D638
ExxonMobil LL 6235 Injection Molding Resin  (discontinued **)
LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in ..
Tensile Strength, Yield 11.00 MPa
1595 psi
ASTM D638
ExxonMobil LL 6235.19 Injection Molding Resin  (discontinued **)
LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in ..