Tensile Strength, Yield 11.76 MPa
1705 psi
ASTM D412
Elastocon TPE Technologies Elastocon® 8088BL Thermoplastic Elastomer
Elastocon® 8088BL is a black lubricated thermoplastic elastomer formulated for applications that require high impact resistance and a reduced coefficient of friction. Elastocon® 8088BL is well sui..