Polymer Property : Tensile Strength, Yield = 115 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 - 115 MPa
6530 - 16700 psi
Average value: 76.5 MPa Grade Count:6
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Tensile Strength, Yield 75.0 - 115 MPa
10900 - 16700 psi
Average value: 97.9 MPa Grade Count:28
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Tensile Strength, Yield 1.06 - 115 MPa
154 - 16700 psi
Average value: 63.1 MPa Grade Count:10
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..