Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 655 - 790 MPa | 95000 - 115000 psi | |
Materion Brush 60™ 3/4 HT Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation afte.. |
|||
Tensile Strength, Yield | 689 - 793 MPa | 100000 - 115000 psi | 0.2% offset |
Eagle Brass 519 Phosphor Bronzes 6%, Extra Spring Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |