Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1060 - 1170 MPa | 154000 - 170000 psi | Solution Annealed & Aged |
Materion Beryllium Copper Alloy 245C Castings (UNS C82600) Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula.. |
|||
Tensile Strength, Yield | 1060 - 1170 MPa | 154000 - 170000 psi | Solution Annealed & Aged |
Materion Beryllium Copper Alloy 245CT Castings (UNS C82600) Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula.. |