Polymer Property : Tensile Strength, Yield = 1196 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.246 MPa
1196 psi
ASTM D412
Elastocon TPE Technologies Elastocon® 2880L Thermoplastic Elastomer
Elastocon® 2880L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2880L is FDA compliant and well s..