Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.7 MPa
1840 psi
ASTM D412
Precision Polymer Engineering V90B Fluoroelastomer Compound
Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M5HK910, A1-11, B38, EF31, EO78, F15, Z1. Where Z1 = compression s..
Tensile Strength, Yield 12.7 MPa

@Thickness 3.20 mm
1850 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOL ED1045D TPO, Thermoplastic Elastomer
Description: Injection Molding, TPO, Thermoplastic Elastomer, Soft TouchApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 1333-86-4, 25087-34-7 and 14807-96-6Information provided..
Tensile Strength, Yield 12.7 MPa
1850 psi
at 100% elongation; ASTM D412
Lubrizol Estane® S195A Thermoplastic Polyurethane
Type: Estane® S195A is a Shore 95A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, ..
Tensile Strength, Yield 12.7 MPa
1840 psi
DIN EN ISO 527
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy
Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato..
Tensile Strength, Yield 12.7 MPa
1840 psi
after aging 1 week @ 135°C; ASTM D638
Trelleborg Horda Cable E8502 Strippable Semiconductive Shielding
E8502 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8502 meets the requirements as bel..
Tensile Strength, Yield 12.7 MPa
1840 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-3890E Thermoplastic Elastomer - SBC  (discontinued **)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..