Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1214 MPa @Strain 0.200 % |
176100 psi @Strain 0.200 % |
|
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 40% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Tensile Strength, Yield | 1214 MPa @Strain 0.200 %, Temperature 371 °C |
176100 psi @Strain 0.200 %, Temperature 700 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 33%, Aged 565°C/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Tensile Strength, Yield | 1214 MPa @Strain 0.200 %, Temperature 426 °C |
176100 psi @Strain 0.200 %, Temperature 799 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 33%, Aged 565°C/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |